N2 - Present study deals the surface morphology and structural composition analysis of alkali (NaOH) treated 2.5% 5.0% and 7.5 wt% Ensete stem fiber obtained from the Ethiopian Ensete ventricosum plant. Treated Ensete fibers reinforced unsaturated polyester (UP) composites were characterized in terms of tensile, flexural, surface morphology and dynamic mechanical properties. Mechanical test results revealed that 5.0 wt% alkali treated Ensete fibers/UP composites showed 14.5% and 43.5% increase in flexural strength and Young's modulus respectively, with relative to untreated Ensete fibers/UP composites. Storage and loss modulus value also highest for 5.0 wt% alkali treated Ensete fibers/UP composites. Moreover, a positive shift in glass transition temperature (Tg) of composites after alkali treatment and tensile fracture surface morphology indicates better interfacial interaction in treated Ensete fibers/UP composites. Overall we concluded that 5.0 wt% treated Ensete fibers satisfactorily and effectively improved mechanical, morphological and dynamic properties of UP for various engineered and hi-tech applications.
AB - Present study deals the surface morphology and structural composition analysis of alkali (NaOH) treated 2.5% 5.0% and 7.5 wt% Ensete stem fiber obtained from the Ethiopian Ensete ventricosum plant. Treated Ensete fibers reinforced unsaturated polyester (UP) composites were characterized in terms of tensile, flexural, surface morphology and dynamic mechanical properties. Mechanical test results revealed that 5.0 wt% alkali treated Ensete fibers/UP composites showed 14.5% and 43.5% increase in flexural strength and Young's modulus respectively, with relative to untreated Ensete fibers/UP composites. Storage and loss modulus value also highest for 5.0 wt% alkali treated Ensete fibers/UP composites. Moreover, a positive shift in glass transition temperature (Tg) of composites after alkali treatment and tensile fracture surface morphology indicates better interfacial interaction in treated Ensete fibers/UP composites. Overall we concluded that 5.0 wt% treated Ensete fibers satisfactorily and effectively improved mechanical, morphological and dynamic properties of UP for various engineered and hi-tech applications.
KW - Alkali treatment
KW - Dynamic mechanical properties
KW - Ensete fibers
KW - Glass transition temperature
KW - Mechanical test
KW - Unsaturated polyester resin
UR - http://www.scopus.com/inward/record.url?scp=85054008262&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85054008262&partnerID=8YFLogxK
U2 - 10.1016/j.compstruct.2018.09.043
DO - 10.1016/j.compstruct.2018.09.043
M3 - Article
AN - SCOPUS:85054008262
SN - 0263-8223
VL - 207
SP - 589
EP - 597
JO - Composite Structures
JF - Composite Structures
ER -